Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A30A Polyether Prepolymer This room-temperature-curable polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this s.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Pot Life | 10.0 - 15.0 min @Temperature 20.0 °C |
10.0 - 15.0 min @Temperature 68.0 °F |
|
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Pot Life | 10.0 - 15.0 min @Temperature 20.0 °C |
10.0 - 15.0 min @Temperature 68.0 °F |
|
Permabond ET515 Epoxy Resin PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A80E High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Pot Life | 12.0 - 15.0 min @Temperature 25.0 °C |
12.0 - 15.0 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2552 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |