Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 10 - 15 min | 10 - 15 min | Mass: 50g |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Pot Life | 8.0 - 15 min | 8.0 - 15 min | Time before parts must be mated |
Lord Adhesives 7542C Two-Component Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 12 - 15 min | 12 - 15 min | |
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works. |
|||
Pot Life | 10 - 15 min | 10 - 15 min | 100 gram batch |
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven.. |
|||
Pot Life | 10 - 15 min | 10 - 15 min | 100 gram mass |
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Pot Life | 14 - 15 min @Temperature 24.0 °C |
14 - 15 min @Temperature 75.2 °F |
1/2 lb mass |
BCC Products BC 5003 Epoxy Laminating System BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive fo.. |
|||
Pot Life | 12 - 15 min @Temperature 24.0 °C |
12 - 15 min @Temperature 75.2 °F |
|
BCC Products BC 8880 Polyurethane Elastomer Surface Coat BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br.. |
|||
Pot Life | 10 - 15 min | 10 - 15 min | Mass: 50g |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Pot Life | 10 - 15 min | 10 - 15 min | Mass: 50g; TM R050-19 |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |