Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 30.0 - 45.0 min @Temperature 20.0 °C |
30.0 - 45.0 min @Temperature 68.0 °F |
|
Permabond ET536 Epoxy Resin PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
|
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas.. |
|||
Pot Life | 30.0 min @Temperature 23.9 °C |
30.0 min @Temperature 75.0 °F |
|
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
|
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6136 Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
100 grams |
Trelleborg Emerson & Cuming Eccobond® 24 LV General Purpose Catalyst Emerson & Cuming 24 LV Eccobond® General Purpose CatalystFaster curing, shorter working life version of 23 LV. Recommended for small mass castings due to higher exotherm. Cure Type: Room Temp or He.. |
|||
Pot Life | 30.0 min @Temperature 80.0 °C |
30.0 min @Temperature 176 °F |
|
Loctite® 3143 Deep Potting Epoxy PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies. For .. |
|||
Pot Life | 30.0 min @Temperature 80.0 °C |
30.0 min @Temperature 176 °F |
|
Loctite® 3166 Deep Potting Epoxy PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies.For e.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) FR-1046 / EA-02 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) RN-1000 / EA-02 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) RN-1000 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) RN-1200 / EA-02 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 30.0 min @Temperature 25.0 °C |
30.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) RN-1210 / EA-02 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | <= 30.0 min @Temperature 25.0 °C |
<= 30.0 min @Temperature 77.0 °F |
100 g |
Armstrong A-1/A Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Pot Life | <= 30.0 min @Temperature 25.0 °C |
<= 30.0 min @Temperature 77.0 °F |
100 g |
Armstrong A-2/A Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Pot Life | <= 30.0 min @Temperature 25.0 °C |
<= 30.0 min @Temperature 77.0 °F |
100 g |
Armstrong A-4/A Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |
|||
Pot Life | <= 30.0 min @Temperature 25.0 °C |
<= 30.0 min @Temperature 77.0 °F |
100 g |
Armstrong A-5/A Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Pot Life | <= 30.0 min @Temperature 25.0 °C |
<= 30.0 min @Temperature 77.0 °F |
100 g |
Armstrong C-1/A Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Pot Life | 30.0 min | 30.0 min | uncured |
Atom Adhesives AA-BOND 2104 Epoxy Adhesive AA-BOND 2104 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
Pot Life | 30.0 min | 30.0 min | uncured |
Atom Adhesives AA-BOND 2123 Epoxy Adhesive AA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. AA-BON.. |
|||
Pot Life | 30.0 min | 30.0 min | uncured |
Atom Adhesives AA-BOND 2153 Epoxy Adhesive AA-BOND 2153 is a thixotropic (smooth paste) thermal conductive epoxy system that passes the NASA Outgassing Specification. It is used for staking transistors, diodes, resistors, integrated circuits.. |
|||
Pot Life | 30.0 min | 30.0 min | uncured |
Atom Adhesives AA-BOND G298 Epoxy Adhesive AA-BOND G298 is a two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Appearance: Resin: Brown, Hardener: Dark Bro.. |
|||
Pot Life | 30.0 - 45.0 min @Temperature 25.0 °C |
30.0 - 45.0 min @Temperature 77.0 °F |
1-2 lbs |
Abatron AboCast/AboCure 4-4/50-12 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: FastBest rigid, chemical, and hea.. |
|||
Pot Life | 30.0 min | 30.0 min | |
Atom Adhesives AA-BOND 2112 Epoxy Adhesive AA-BOND 2112 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
Pot Life | 30.0 min | 30.0 min | |
Atom Adhesives AA-BOND 2116 Epoxy Adhesive AA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronics, aerospace, and industrial applications where.. |
|||
Pot Life | 30.0 min | 30.0 min | |
Atom Adhesives AA-BOND F156 Epoxy Adhesive AA-BOND F156 is a black, solvent free thixotropic epoxy recommended for high quality photographic industry, laminating, production and repair applications where a room temperature cure optically opa.. |
|||
Pot Life | 30.0 - 40.0 min @Temperature 20.0 °C |
30.0 - 40.0 min @Temperature 68.0 °F |
|
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |
|||
Pot Life | 30.0 min | 30.0 min | uncured |
Atom Adhesives AA-BOND 2101 Epoxy Adhesive AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and el.. |