Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 12 - 15 min | 12 - 15 min | |
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works. |
|||
Pot Life | 12 min | 12 min | |
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Pot Life | >= 12 min | >= 12 min | 200 gram mass |
Master Bond Supreme 46HT-2 Toughened, High Shear and Peel Strength Adhesive Description: Master Bond Supreme 46HT-2 is a two component epoxy adhesive featuring an attractive balance of good shear and peel strengths for high performance structural bonding and coating suitabl.. |
|||
Pot Life | 12 - 14 min | 12 - 14 min | |
Abatron AboWeld/AboCure 7812-2 Thixotropic Epoxy AboWeld/AboCure 7812-2 is an underwater and cold-weather structural and dielectric adhesive paste. It is a 2-component thixotropic epoxy compound for dry, wet, and cold applications. It has many spe.. |
|||
Pot Life | 12 min @Temperature 24.0 °C |
12 min @Temperature 75.2 °F |
1 lb. mass |
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w.. |
|||
Pot Life | 12 - 14 min @Temperature 24.0 °C |
12 - 14 min @Temperature 75.2 °F |
mass dependent |
BCC Products BC 8782 Urethane Casting BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi.. |
|||
Pot Life | 12 - 15 min @Temperature 24.0 °C |
12 - 15 min @Temperature 75.2 °F |
|
BCC Products BC 8880 Polyurethane Elastomer Surface Coat BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br.. |