Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 11 - 18 min | 11 - 18 min | Time before parts must be mated |
Lord Adhesives 7545D Two-Component, Equal-Mix, Non-Sag Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 11 min | 11 min | |
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Pot Life | 11 min | 11 min | |
Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |