Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A30A Polyether Prepolymer This room-temperature-curable polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this s.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Pot Life | 10.0 - 13.0 min | 10.0 - 13.0 min | |
Northstar Polymers MPP-D65A Polyether Base Polyurethane Resin MPP-D65A is a polyether base 2-component polyurethane resin casting system for molding and potting applications. It has a long pot-life and gradual curing pattern to provide easier handling for mol.. |
|||
Pot Life | 10.0 - 15.0 min @Temperature 20.0 °C |
10.0 - 15.0 min @Temperature 68.0 °F |
|
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Pot Life | 10.0 - 15.0 min @Temperature 20.0 °C |
10.0 - 15.0 min @Temperature 68.0 °F |
|
Permabond ET515 Epoxy Resin PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Pot Life | 10.0 - 12.0 min @Temperature 25.0 °C |
10.0 - 12.0 min @Temperature 77.0 °F |
|
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Pot Life | 10.0 - 15.0 min | 10.0 - 15.0 min | |
Northstar Polymers MPP-A80E High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Pot Life | 10.0 - 130000 min | 10.0 - 130000 min | Average value: 5130 min Grade Count:105 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Pot Life | 10.0 min @Temperature 23.9 °C |
10.0 min @Temperature 75.0 °F |
|
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black Information provided by ITW Devcon |
|||
Pot Life | 10.0 min @Temperature 23.9 °C |
10.0 min @Temperature 75.0 °F |
|
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black Information provided by ITW Devcon |
|||
Pot Life | 10.0 min @Temperature 23.9 °C |
10.0 min @Temperature 75.0 °F |
|
ITW Devcon Rubber Repair / Castable Urethane Cable Cast FR, Black Information provided by ITW Devcon |
|||
Pot Life | 10.0 min @Temperature 23.0 °C |
10.0 min @Temperature 73.4 °F |
|
Loctite® 3171 Deep Potting Polyurethane PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies.For e.. |
|||
Pot Life | 10.0 min @Temperature 23.0 °C |
10.0 min @Temperature 73.4 °F |
|
Loctite® 3180 Deep Potting Polyurethane PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies. For .. |
|||
Pot Life | 10.0 min @Temperature 25.0 °C |
10.0 min @Temperature 77.0 °F |
0.5 lbm |
Cytec EN-8 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Pot Life | <= 10.0 min | <= 10.0 min | |
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia Two-part, quick-set ceramic for small parts. |