Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 170 - 210 °C | 338 - 410 °F | Average value: 195 °C Grade Count:10 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Head Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion Molding |
Kolon ELLAS K-260D Thermoplastic Polyurethane ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion Molding |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEMâ€; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki.. |
|||
Head Temperature | 190 - 210 °C | 374 - 410 °F | |
Borealis Borcoat™ HE3450 Black High Density Polyethylene Top Coat for Steel Pipe Coating Borcoat HE3450 is a black, high-density polyethylene (HDPE) produced with the advanced Borstar technology, providing the material with especially well melt strength and extrudability. Also its mech.. |
|||
Head Temperature | 190 - 210 °C | 374 - 410 °F | |
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3494-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3410 HDPE for Sewage Pipes Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3470-LS Black HDPE Compound for Pressure Pipes Borstar HE3470-LS is a black, high density polyethylene compound classified as an MRS 8.0 material (PE80) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding .. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3494-LS Dark Blue High Density Polyethylene for Drinking Water Pipes Borstar HE3494-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combinat.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3492-LS Yellow-Orange High Density Polyethylene for Natural Gas Pipes Borstar HE3492-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina.. |
|||
Head Temperature | 185 - 210 °C | 365 - 410 °F | Average value: 196 °C Grade Count:6 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | Average value: 205 °C Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | Average value: 204 °C Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding.. |
|||
Head Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® ME3444 Blue Medium Density Polyethylene for Drinking Water Pipes Borstar 3444 is a blue, bimodal, medium density polyethylene classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. A combination of pigments and stabilizers is incl.. |