Polymer Property : Head Temperature = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 190 - 200 °C
374 - 392 °F
Average value: 195 °C Grade Count:4
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry Parts Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon.
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon.
Head Temperature 185 - 200 °C
365 - 392 °F
Extrusion Molding
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon.
Head Temperature 185 - 200 °C
365 - 392 °F
Extrusion Molding
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane
ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.