Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 180 - 190 °C | 356 - 374 °F | |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 180 - 190 °C | 356 - 374 °F | |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 180 - 190 °C | 356 - 374 °F | |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 180 - 190 °C | 356 - 374 °F | |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 185 - 190 °C | 365 - 374 °F | |
Equate EMDA-6200 HDPE Blow Molding Resin EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for .. |