Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 260 - 280 °C | 500 - 536 °F | |
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |