Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 170 - 210 °C | 338 - 410 °F | Average value: 195 °C Grade Count:10 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Head Temperature | 170 - 180 °C | 338 - 356 °F | Extrusion Molding |
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon. |
|||
Head Temperature | >= 170 °C | >= 338 °F | |
Borealis Casico™ FR4807 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing Casico FR4807 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4804 offers a unique combination of good extrusion pr.. |
|||
Head Temperature | >= 170 °C | >= 338 °F | |
Borealis Casico™ FR4804 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing Borstar FR4804 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4804 offers a unique combination of good extrusion p.. |