Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Head Temperature | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Head Temperature | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |