Die Cooling Temperature 30.0 - 50.0 °C
86.0 - 122 °F
water cooling
Borealis HE4872 High Density Polyethylene
HE4872 is a HDPE compound for solid insulation of symmetric data cable at high extrusion speed. Applications: high frequency data transmission cables, outer skin of foam-skin constructions. Specif..