Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.0760 - 0.130 cm | 0.0299 - 0.0512 in | |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |