Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.180 - 0.250 cm | 0.0709 - 0.0984 in | |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Die Opening | 0.180 - 0.250 cm | 0.0709 - 0.0984 in | |
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring .. |
|||
Die Opening | 0.180 - 0.250 cm | 0.0709 - 0.0984 in | |
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en.. |
|||
Die Opening | 0.180 - 0.250 cm | 0.0709 - 0.0984 in | |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu.. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |
|||
Die Opening | >= 0.180 cm | >= 0.0709 in | |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |
|||
Die Opening | 0.180 - 0.250 cm | 0.0709 - 0.0984 in | Blown Film Extrusion |
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s.. |
|||
Die Opening | 0.180 - 0.250 cm | 0.0709 - 0.0984 in | Blown Film Extrusion |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |
|||
Die Opening | 0.180 - 0.250 cm @Temperature 200 - 220 °C |
0.0709 - 0.0984 in @Temperature 392 - 428 °F |
Blown Film Extrusion |
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve.. |
|||
Die Opening | 0.180 - 0.250 cm @Temperature 200 - 220 °C |
0.0709 - 0.0984 in @Temperature 392 - 428 °F |
Average value: 0.215 cm Grade Count:1 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |