Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.0640 cm | 0.0252 in | |
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Die Opening | 0.0640 cm | 0.0252 in | |
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra.. |
|||
Die Opening | 0.0640 cm | 0.0252 in | |
Chevron Phillips MarFlex® 7120B LLDPE Blown & Cast Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Die Opening | 0.0640 - 0.280 cm | 0.0252 - 0.110 in | Average value: 0.0991 cm Grade Count:14 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |