Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LL1091 LLDPE
(discontinued **) Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LL1091-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LM112-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LM115-B LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LL1091-AS LLDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | Average value: 0.169 cm Grade Count:6 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | Average value: 0.172 cm Grade Count:13 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LL1092-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LM203-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LM213-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Die Opening | 0.0810 - 0.254 cm | 0.0319 - 0.100 in | |
M. Holland Company MAGMA® LM311-D LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |