Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.0760 - 0.280 cm | 0.0299 - 0.110 in | Average value: 0.164 cm Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Die Opening | 0.0760 - 0.130 cm | 0.0299 - 0.0512 in | |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |