Processing Properties Metric English Comments
Die Opening 0.0640 cm
0.0252 in
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Die Opening 0.0640 cm
0.0252 in
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra..
Die Opening 0.0640 cm
0.0252 in
Chevron Phillips MarFlex® 7120B LLDPE Blown & Cast Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Die Opening 0.0640 - 0.280 cm
0.0252 - 0.110 in
Average value: 0.0991 cm Grade Count:14
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade