Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 152 MPa | 7500 - 22000 psi | Average value: 100 MPa Grade Count:16 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |