Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FFSL 7041 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FFSL 7051 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6061 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2010 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2040 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2060 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/05 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/07 Liquid Silicone Rubber - Specialty Coating Conductive coating - Physical Properties are subject to the substrate that is used. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2540 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 LV Liquid Silicone Rubber - Low Volatile / High Tear This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2660 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2661 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2670 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2670FC High Productivity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 3485/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 3596/30 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4670 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7005 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7080 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 3386/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Silopren™ LSR 3386/30 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |