Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT5100-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T20P100-01EG 20% Talc Reinforced Polypropylene, General Purpose Black, Extrusion Grade Applications: Consumer goodsAutomotive componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP522-473 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZU5A Dark Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP525-01 30% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Center consolesInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |