Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass beads and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B GB 30 PBT, 30% glass beads FeaturesPBT for injection moulding, chemically reinforced with 30% glass beads. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Injection Pressure | 40.0 - 100 MPa | 5800 - 14500 psi | 3-15 sec |
Zhejiang Juner 301-G0 Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |