Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 1000 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 1501 Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 1501E Description: Extrusion GradeInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 1502 Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3500 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3500 Natural 1050 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501 GF-30 Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501 Natural 1050 Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 3501 SHF Description: Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501E Natural 1000 S Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4001H3F Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4003HH Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4500R Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 7500E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 7502 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 9500B Description: Blow Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 9502 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 9502E Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS TM 40 Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS VP-11 SHF Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers TR 5000 Description: Transparent ABSInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501 GF-20 Description: Reinforced Grade, 20%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS VP-11 Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |