Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B1 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Ineos ABS Centrex® 833 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Injection Pressure | 60.0 - 90.0 MPa | 8700 - 13100 psi | |
Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl.. |