Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 58.84 - 98.1 MPa | 8534 - 14200 psi | First |
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Injection Pressure | 58.84 - 137.3 MPa | 8534 - 19910 psi | |
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding High flowability gradeParticularly recommended for complicated profiles or large and thin wall partsFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface har.. |
|||
Injection Pressure | 58.84 - 137.3 MPa | 8534 - 19910 psi | |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Injection Pressure | 58.84 - 88.26 MPa | 8534 - 12800 psi | Second |
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Injection Pressure | 58.84 - 88.26 MPa | 8534 - 12800 psi | Second |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Injection Pressure | 58.84 - 88.26 MPa | 8534 - 12800 psi | Second |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Injection Pressure | 58.84 - 98.1 MPa | 8534 - 14200 psi | First |
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Injection Pressure | 58.84 - 98.1 MPa | 8534 - 14200 psi | First |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Injection Pressure | 58.84 - 98.1 MPa | 8534 - 14200 psi | First |
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Injection Pressure | 58.84 - 98.1 MPa | 8534 - 14200 psi | First |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |