Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 152 MPa | 7500 - 22000 psi | Average value: 100 MPa Grade Count:16 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
Mitsubishi Iupilon® H2000R 23 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 51.7 - 124 MPa | 7500 - 18000 psi | |
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |