Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural Applications: BracketsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M20P101-01 20% Mica Reinforced Polypropylene, Black Applications: Radiator air bafflesHVAC ductworkClose-out and filler panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products F24-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Head lamp housingsBracketsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |