Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free
(discontinued **) Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed
(disc Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage
(discontinued **)& Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 14600 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, low specific gravity.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a part of Hexion in 2005.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak .. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Contact strips.Information provided by Bak AGBak AG became a part of Hexion in 20.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good .. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 83 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Switch covers, rolls, handle casings.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed
&n Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte.. |