Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 1.38 - 103 MPa | 200 - 15000 psi | Average value: 66.9 MPa Grade Count:17 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1458 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1561 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1579D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1695L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1838-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2103 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2197 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2239 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2315 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2334-R2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1366A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1426A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2740L3-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® OBC 4665A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1446G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2448G Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2570A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2575A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-94-T0586C-113 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2580A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Uniprene® UN-2533A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2730 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP 1210A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |