Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 100 - 150 MPa | 14500 - 21800 psi | |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |
|||
Injection Pressure | 100 - 150 MPa | 14500 - 21800 psi | |
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-.. |
|||
Injection Pressure | 100 MPa | 14500 psi | |
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Injection Pressure | 100 MPa | 14500 psi | |
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Dry, 40% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Injection Pressure | 100 MPa | 14500 psi | |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Injection Pressure | 100 - 140 MPa | 14500 - 20300 psi | |
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Injection Pressure | 100 MPa | 14500 psi | |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Injection Pressure | 100 MPa | 14500 psi | |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Injection Pressure | 100 MPa | 14500 psi | |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Injection Pressure | 100 MPa | 14500 psi | |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Injection Pressure | 100 - 140 MPa | 14500 - 20300 psi | |
Plastcom SLOVALEN PH 49 GF 60 PP reinforced with 60% glass fibre Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered.. |