Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PCSP0014 GREY Polycarbonate, Stainless Steel Fiber, EMI Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 612G10-L Nylon 612, 10% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6253 Nylon 6, High Impact Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR2025 Nylon 66, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol CP-MF-9 Acetal Copolymer Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBTG30-L Polybutylene Terephthalate, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PC010-L FR Polycarbonate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0004 Polycarbonate Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol R60G33HSL Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol TPU2087AFR Polyurethane Elastomer, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPSS0007 Polyphenylene Sulfide, Glass Fiber and Mineral Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 66G33-L Nylon 66, 33% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® S175A Thermoplastic Polyurethane Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |