Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Plastcom SLOVAMID 6 GF 15 FRG 2 LW PA6, 15% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 960°.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
SABIC MG500026 Linear Low Density Polyethylene for Compounding Product Description: MG500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding applications. It is in the powder form and h.. |
|||
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
SABIC M200056 High Density Polyethylene for Injection Molding Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
Gromax PBT 1100-211XG Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
Zhejiang Juner PC Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 40.0 - 100 MPa | 5800 - 14500 psi | |
Beijing Chemical Industry KAIFA® 301-G0 PBT Resin Flame retardant, folding enduranceInformation provided by Beijing Chemical Industry Research Institute (Group) |