Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC10P100-00 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G20P252-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Black Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products CC20P100-01 20% Calcium Carbonate Reinforced Polypropylene, Black Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |