Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T470A Thermoplastic Polyurethane Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PA131 Nylon 66, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 60G33HSL Nylon 6, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR7039G30 Nylon 6, 30% Glass Fiber, bondable to TPU Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol CP-MF-9 Acetal Copolymer Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA211 Nylon 6, General Purpose Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA211G50 Nylon 6, 50% Glass Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA213G33 Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA233G13 Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0011HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBT1100S Polybutylene Terephthalate, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0006GY-371 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0015 Polycarbonate, Carbon Fiber Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6608G43 Nylon 66, 43% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR7039G15 Nylon 6, 15% Glass Fiber, bondable to TPU Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PURSP0005 Polyurethane Elastomer, Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA111G30IF Nylon 66, 30% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |