Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 63.74 - 93.16 MPa | 9245 - 13510 psi | First |
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Injection Pressure | 63.74 - 93.16 MPa | 9245 - 13510 psi | First |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Injection Pressure | 63.74 - 93.16 MPa | 9245 - 13510 psi | First |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |