Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ Electro 242-3 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FFSL 7031 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FFSL 7051 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7641 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6010 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2003 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2050 Liquid Silicon Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2631 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2660 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2671 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 3596/30 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4020 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4070 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4080 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem 475-860N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB860EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-975 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-845B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |