Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 41.4 - 103 MPa | 6000 - 15000 psi | Average value: 83.6 MPa Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Injection Pressure | 41.4 - 62.1 MPa | 6000 - 9000 psi | Second |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 41.4 - 62.1 MPa | 6000 - 9000 psi | Second |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 41.4 - 82.7 MPa | 6000 - 12000 psi | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Injection Pressure | 41.4 - 82.7 MPa | 6000 - 12000 psi | Injection Molding |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Injection Pressure | 41.4 - 82.7 MPa | 6000 - 12000 psi | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Injection Pressure | 41.4 - 82.7 MPa | 6000 - 12000 psi | Secondary |
Clariant Renol PCSP0008BK Polycarbonate, ESD Protection Data provided by Clariant Masterbatches |
|||
Injection Pressure | 41.4 - 82.7 MPa | 6000 - 12000 psi | Secondary |
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 41.4 - 74.5 MPa | 6000 - 10800 psi | Secondary |
Clariant Renol PPA1100G50 Polyphthalamide, 50% Glass Fiber Data provided by Clariant Masterbatches |
|||
Injection Pressure | 41.4 - 74.5 MPa | 6000 - 10800 psi | Secondary |
Clariant Renol PPOSP0001 Polyphenylene Oxide, Mineral Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 41.4 - 74.5 MPa | 6000 - 10800 psi | Secondary |
Clariant Renol PPSP0017 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Injection Pressure | 41.4 - 74.5 MPa | 6000 - 10800 psi | Secondary |
Clariant Renol PPSSP0008 Polyphenylene Sulfide, Carbon Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 41.4 - 74.5 MPa | 6000 - 10800 psi | Secondary |
Clariant Renol PPA1100G60 Polyphthalamide, 60% Glass Fiber Data provided by Clariant Masterbatches |
|||
Injection Pressure | 41.4 - 138 MPa | 6000 - 20000 psi | Average value: 86.8 MPa Grade Count:57 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |