Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Polykemi AB POLYelast TPE HJ753 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP1001F Polypropylene Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP6020F Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP EIP12030F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH GF3045 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH GK8040 Polypropylene Homopolymer, Glass Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH B8065 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH BK901010 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH GF5010 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH GF8020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH K5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 100 MPa | 5800 - 14500 psi | |
Zhejiang Juner JEPPB005 High Glossy PP Applications: Shell of Air ConditionerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Pressure | 40.0 - 100 MPa | 5800 - 14500 psi | |
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH T20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPH TS8020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Polykemi AB POLYfill PPHC K1035 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |