Processing Properties Metric English Comments
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL HI-525 High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N109-AS Antistatic POM, Unreinforced, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N127-AS Antistatic POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N145-02 General Purpose POM, Unreinforced, Externally Lubricated, Ultra High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL VC127-LD Antistatic POM, Unreinforced, High Flow, For VCR Reels
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 49.03 MPa
4978 - 7111 psi
Second
LG Chemical Lupox® GP-1006F General Purpose PBT, Unreinforced, Flame Retardant, Non-Bleed
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 34.32 - 49.03 MPa
4978 - 7111 psi
Second
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 34.32 - 49.03 MPa
4978 - 7111 psi
Second
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 34.32 - 49.03 MPa
4978 - 7111 psi
Second
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 34.32 - 49.03 MPa
4978 - 7111 psi
Second
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 34.32 - 68.65 MPa
4978 - 9957 psi
Second
LG Chemical LUCEL FW-700A Friction and Wear Resistant POM, Polymeric Wear Additive
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Injection Pressure 34.32 - 49.03 MPa
4978 - 7111 psi
Second
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Copyright © lookpolymers.com All Rights Reserved