Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATG 112 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 157 Phenolic Molding Long glass fiber Filler, Compression Molded Characteristics:Shock resistant ( High impact strength )Very good mechanical strengthGood dielectric strengthLow water absorptionLow shrinkageColor-pale brown, black, dark brown, green etc.Medium/st.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Injection Pressure | 15.68 - 34.3 MPa | 2274 - 4970 psi | Mold Pressure |
Amity Thermosets ATS 766 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BrownMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |