| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® 3385A Polyurethane Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® 790 Polyurethane Extrusion- and injection molding gradehigh mechanical strengthApplicationToothed beltsProfilesInjection molded engineering partsPreprocessingMax. Water content |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® 9385 Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 1080A Polyurethane injection molding gradefree from plasticizershard - soft systemsTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covest.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 1485A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldingvery large processing windowhigh melt stabilityBeadsApplicationBellowsHosesnon-reinforcedProfilesInjection molded engineering.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 2586A Polyurethane Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentBeadsApplicationBlown filmsPreprocessingMax. Water co.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 2590A Polyurethane Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationBlown filmsPreprocessingMax. Water content.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 2786A Polyurethane Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 2792A Polyurethane Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 3491A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldinghigh mechanical strengthhigh melt stabilityApplicationBlow moldingProfilesInjection molded engineering partsPreprocessingMax... |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 3660DU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 3690AU Polyurethane Extrusion- and injection molding gradehydrolysis-stabilisedwith special UV stabilizerswith release agenttransparent up to 6 mm wall thicknessgood wear resistanceApplicationSports shoe solesFilmsHose.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 3695AU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 5080A Polyurethane injection molding gradeimproved microbial resistanceImproved hydrolysis resistanceApplicationSealsmembraneshard - soft systemsPreprocessingMax. Water content |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 6065A Polyurethane injection molding gradefree from plasticizersvery good hydrolysis and microbial resistancevery short cycle timesApplicationhard - soft systemsShoe solesPreprocessingMax. Water content |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 8798A Polyurethane injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9095AU Polyurethane injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood wear resistancelow warpargeshort cycle timesApplicationEar-tagsPreprocessingMax. Water content |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9370A Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9380A Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9392AU Polyurethane Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationHosesnon-reinforcedCable sheathingsProfilesTe.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9395AU Polyurethane Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationPneumatic hosesProfilesCable sheathingsInject.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9650DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedAs of .. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9659DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9662DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® DP 9665DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPneuma.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® W DP 85085A Polyurethane injection molding gradeno yellowing under the action of UV lightimproved microbial resistancegood low-temperature flexibilityImproved hydrolysis resistanceApplicationautomotive interior applications.. |
|||
| Ejection Temperature | 50.0 °C | 122 °F | |
| Covestro Desmopan® W DP 89051D Polyurethane PreprocessingMax. Water content |
|||