Processing Properties | Metric | English | Comments |
---|---|---|---|
Ejection Temperature | 120 °C | 248 °F | |
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend
(discontinued **) Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay.. |
|||
Ejection Temperature | 120 °C | 248 °F | |
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade Flame retardant extrusion gradeVicat/B 120 temperature = 115 °Cgood extrusion and vacuum-forming behaviourUL-listing 94 V-0 (1.5 mm)halogen-free according to DIN VDE 0472-815glow wire temperature (.. |
|||
Ejection Temperature | 120 °C | 248 °F | |
Covestro Bayblend® T65 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content |
|||
Ejection Temperature | 120 °C | 248 °F | |
Covestro Bayblend® T65 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content |
|||
Ejection Temperature | 120 °C | 248 °F | |
Covestro Bayblend® KU 1-1446* Polycarbonate + ABS Developmental productGrade with improved low-temperature impact strength and petrol resistance for automotive partsin version BBS904 suitable for extrusion/extrusion blow molding and electroplating .. |