Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 0.250 hour @Temperature 21.0 °C |
0.250 hour @Temperature 69.8 °F |
Touch |
Chesterton 752 Cold Galvanizing Compound Description: Chesterton® 752 Cold Galvanizing Compound functions both as a zinc rich primer or final coating for ferrous metals and their welds exposed to atmospheric or corrosive conditions. The p.. |
|||
Dry Time | 0.250 hour @Temperature 24.0 °C |
0.250 hour @Temperature 75.2 °F |
then 45 minutes at 65°C |
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C.. |