Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 150P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 650P PolyEtherEtherKetone High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Info.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 90P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Dry Time | 3.00 hour @Temperature 180 °C |
3.00 hour @Temperature 356 °F |
|
Victrex® ST™ P45 PolyEtherKetoneEtherKetoneKetone (PEKEKK), High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.Information Provid.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Dry Time | 3.00 hour @Temperature 150 °C |
3.00 hour @Temperature 302 °F |
|
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |