Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load b.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MCP-V40A Polyurethane Gel MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two.. |
|||
Processing Temperature | 18.3 - 32.2 °C | 65.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPA-A30B Mold-Making Resin MPA-A30B is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A30A Polyether Prepolymer This room-temperature-curable polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this s.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A50A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A90A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-D80B Rigid Polyurethane MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured pr.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-R07B Polyurethane Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled
(discontinued **) Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPS-M23B Room-Temperature Curable Microcellular Foam This foam polyurethane formulation is designed to yield closed-cell microcellular foam by either hand-mixing or machine casting method at room temperature. The components are liquid at room temperat.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-AS1 High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |