Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 271 - 288 °C | 520 - 550 °F | |
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding 33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 271 - 288 °C | 520 - 550 °F | |
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding 43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 271 - 288 °C | 520 - 550 °F | |
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding 50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile Temperature |
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile temperatures |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile temperatures |
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile Temperature |
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile temperatures |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile Temperature |
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile temperatures |
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile Temperature |
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Processing Temperature | 249 - 288 °C | 480 - 550 °F | Profile Temperature |
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | Average value: 277 °C Grade Count:3 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Processing Temperature | 227 - 288 °C | 440 - 550 °F | Average value: 261 °C Grade Count:5 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Processing Temperature | 221 - 288 °C | 430 - 550 °F | Soldering Range |
Lucas-Milhaupt Silvabrite® S™ Lead-Free Solder Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidentl.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 900 Clear Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman 980-05V0 Grey Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Processing Temperature | 266 - 288 °C | 510 - 550 °F | |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |