Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 266 - 287 °C | 511 - 549 °F | |
Shuman SP910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Processing Temperature | 266 - 287 °C | 511 - 549 °F | |
Shuman SP920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Processing Temperature | 266 - 287 °C | 511 - 549 °F | |
Shuman SP930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Processing Temperature | 266 - 287 °C | 511 - 549 °F | |
Shuman SP980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Processing Temperature | 143 - 287 °C | 289 - 549 °F | Injection |
Dyna-Purge® K Purging Compound Designed or a broad range of "Low-Temp" resinsGeneral Description:DYNA-PURGE K is a low-temp, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow nat.. |
|||
Processing Temperature | 143 - 287 °C | 289 - 549 °F | Extrusion |
Dyna-Purge® K Purging Compound Designed or a broad range of "Low-Temp" resinsGeneral Description:DYNA-PURGE K is a low-temp, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow nat.. |