Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 200 - 240 °C | 392 - 464 °F | Barrel Temperature |
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antist.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | |
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Processing Temperature | 200 - 240 °C | 392 - 464 °F | Barrel Temperature |
SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 57MNK10 is a controlled rheology PP grade of medium molecular weight distribution specially developed for producing injection molded articles. This grade has an excellent i.. |
|||
Processing Temperature | 171 - 240 °C | 340 - 464 °F | Average value: 196 °C Grade Count:22 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
IRPC Polimaxx Polene 2300NC Polypropylene Block Copolymer CHARACTERISTICS: MEDIUM FLOW, GOOD IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, FURNITURES, CRATES |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
IRPC Polimaxx Polene 2363LC Polypropylene Block Copolymer CHARACTERISTICS: CONTAIN UV STABILIZER ADDITIVE, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, FURNITURES, CRATES |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
IRPC Polimaxx Polene 2541TC Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT FLOWABILITY, HIGH STIFFNESS, HEAT STABILITY, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING SPECIALLY FOR WASHING TUB, ELECTRICAL APPLIANCES, THIN WALL CONTAINERS |
|||
Processing Temperature | 210 - 240 °C | 410 - 464 °F | injection |
IRPC Polimaxx Polene GP110 Polystyrene APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc. |
|||
Processing Temperature | 160 - 240 °C | 320 - 464 °F | Coatings |
Lucobit Lucofin® 1413 Polyolefin TPO Granules, Dark Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 160 - 240 °C | 320 - 464 °F | Bitumen modification |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Processing Temperature | 160 - 240 °C | 320 - 464 °F | Coatings |
Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 230 - 240 °C | 446 - 464 °F | C3 |
UBE 1026B1 Nylon 6 Homopolymer Film Specialties: Nucleated (High viscosity) Processing: T-die, Air blownApplications: General applicationsInformation provided by UBE. |
|||
Processing Temperature | 230 - 240 °C | 446 - 464 °F | C4 |
UBE 5033FDX27 Air Blown Nylon 6/66 Film Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
Total MDPE 3802 Medium Density Polyethylene, Cable MDPE 3802 is a natural medium density polyethylene particularly suited for colored cable sheathing applications and designed to meet the requirements for telecommunication and power cables (medium a.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | |
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
Fainplast Compounds Ethylplus 600 Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid LDPEInformation provided by Fainplast Compounds.. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
Fainplast Compounds Ethylplus 611 LE Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesExpandable LDPEInformation provided by Fainplast Comp.. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
Fainplast Compounds Ethylplus 621 HD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid HDPEInformation provided by Fainplast Compounds.. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
Fainplast Compounds Ethylplus 623 HD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack HDPE SheathingInformation provided by Fainplast.. |
|||
Processing Temperature | 210 - 240 °C | 410 - 464 °F | Extrusion Range |
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastollan SP 852 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Processing Temperature | 60.0 - 240 °C | 140 - 464 °F | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | Injection molding |
BASF Elastollan C 70 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastollan S 74 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | Average value: 211 °C Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastollan S 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 193 - 240 °C | 380 - 464 °F | Average value: 212 °C Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Processing Temperature | 160 - 240 °C | 320 - 464 °F | Coatings |
Lucobit Lucofin® 1460 Polyolefin TPO Granules, White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |