Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer
(discontinued **) A hard, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has low friction and is especially designed for use as a co-extruded slip-coat layer on weath.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8201-67W228 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8211-65M300 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 281-73MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Processing Temperature | 200 - 230 °C | 392 - 446 °F | Barrel Temperature |
SABIC PP 651H Polypropylene Random Copolymer for PIPE Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical App.. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 199 °C Grade Count:29 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 199 °C Grade Count:8 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | |
IRPC Polimaxx Polene 3342M Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, GOOD FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING, INJECTION STRETCH BLOW MOLDING (ISBM) FOR FOOD CONTAINERS, BOTTLES, HOUSEWARES, CRATES |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucobit® 1221 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Processing Temperature | 160 - 230 °C | 320 - 446 °F | Membranes |
Lucobit Lucofin® 1412-t2 Polyolefin TPO Granules, Light Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t2 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 210 - 230 °C | 410 - 446 °F | |
Taiwan Sheen Soon Sheenthane® D7220 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Processing Temperature | 210 - 230 °C | 410 - 446 °F | |
Bond Laminates TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 M POM Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Extrusion |
BASF Elastollan B 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Injection molding |
BASF Elastollan B 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Injection molding |
BASF Elastollan B 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Processing Temperature | 190 - 230 °C | 374 - 446 °F | Injection |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 200 LS POM Injection molding grade based on Tarnoform 200 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Processing Temperature | 180 - 230 °C | 356 - 446 °F | Resin Temp. |
Beijing Chemical Industry KAIFA® GL3100 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 121-68W228 Thermoplastic Elastomer
(discontinued **) A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion applications and has long te.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 221-87W211 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Processing Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Range |
Arkema Group Pebax® MX 1205 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information prov.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |